Re: Fixing and upgrading an Enterprise 64
Posted: 06 Aug 2026 16:44
If you used PLA it may start to deform as that heatsink gets very toasty, above the PLA glass temperature. PET-G *may* have enough thermal headroom.
We welcome retro users & hardware gurus alike! Come and join the party :)
https://www.exxosforum.co.uk/forum/
Fortunately I was already thinking the same and used PET-G :)stephen_usher wrote: 06 Aug 2026 16:44 If you used PLA it may start to deform as that heatsink gets very toasty, above the PLA glass temperature. PET-G *may* have enough thermal headroom.